Grade SY-65 · technical data from the plant

Black Masterbatch SY-65 — 65% Carbon Black, Carrier-Free Engineering Grade

The top of the concentration range: 65% carbon black, no carrier resin, for ABS, PS and PC modification. Deep jetness with maximum let-down flexibility — technical compounders dilute to wherever the application needs the carbon to be.

65% carbon blackCarrier-free (CB only)Ash <10% (carbon black only)Batch CoA per lotFactory-direct
USD 3.00–6.00 / kgFOB Shenzhen
On quotationminimum order
10–15 daysafter spec confirmation
Lot-by-lot CoA10 release checks

Technical data — SY-65

Typical values from in-house QC. We confirm the contractual spec against your order, with a batch CoA on every shipment.

Black masterbatch SY-65 — typical values
PropertyTypical value
Carbon black content65%
Carrier systemCarrier-free (CB only)
Ash content<10% (carbon black only)
Melt flow rate (190 °C)on request
Moisture<0.50%
Recommended let-down1–3%
Density—
FOB price rangeUSD 3.00–6.00 / kg (FOB)
Minimum orderMinimum order quantities are confirmed in the quotation for this grade and specification (samples free)
Delivery10–15 days after spec confirmation
Packaging25 kg KP or PE bags, 20 bags per pallet
Loading portShenzhen, China
HS code32064900
Quality standardsISO 9001 / 14001 / 45001 plant · batch CoA per lot

Values are typical QC reference data, not contractual specifications — request the full TDS and we send it the same day.

Who this grade is for

Where SY-65 shows up in our export business, and why buyers pick it.

Use case

ABS / PS / PC compounding

Engineering-resin modification where jetness and conductivity thresholds matter.

Use case

High-blackness technical parts

Deep jet surfaces at the lowest possible addition.

Use case

Compounders who set their own let-down

65% concentrate lets you put exactly 0.5%, 1% or 3% carbon into the compound by dosage alone.

Use case

Masterbatch producers

A concentrate to let down into your own carrier system.

Why these numbers

The formulation logic behind the spec sheet — what the chart does not say.

Carrier-free at 65% is the whole point: adding SY-65 to a melt adds carbon black and nothing else. The host resin — ABS, PS, PC — stays the only polymer in the system, so HDT, impact and flow remain exactly what your base compound specifies.

Jetness scales with real carbon in the wall: at 65%, 2% let-down puts 1.3% carbon in the part — the deep-black region where lower grades need 4–5% addition and drag carrier along with it.

Screening and dispersion are the hard part at this loading; the ash ceiling below 10% reflects carbon black purity plus compounding aids only.

Running a 65% grade: what it demands of your line

High loading is bought for what it puts into the part. It is earned on the line — these are the four things that decide whether you get the dispersion you paid for.

1. Drying is not optional at this loading

At 65% the carbon fraction dominates the pellet, and moisture carried in with it shows up in the part faster than it does at 40%. Where a 40% grade might tolerate a marginal hopper, a 65% grade will put bubbles, streaks or a speckle into a visible surface. Dry to the figure on the TDS and keep it dry to the screw.

2. Feeding: expect bridging before you expect under-dosing

Very high carbon loadings make for a denser, sometimes less free-flowing pellet. On vacuum loaders and long flexible runs, bridging at a bend or a receiver is the usual failure — not a starving feeder. If your conveying system is already marginal, test it on this grade before you plan a full campaign.

3. Dispersion is a shear budget, and 65% spends more of it

Dispersing carbon black is work, and the work scales with how much carbon each pellet carries. A twin-screw line with a proper mixing section handles 65% without drama; a single-screw line being asked to do more than it was set up for will deliver a reading that looks like a bad lot but is actually a shear shortfall. If this is your first 65% grade, tell us the machine and we will say plainly whether it is set up for it — that conversation is cheaper than a failed campaign.

4. The let-down calculation becomes the whole game

Because the carrier is gone, addition ratio maps almost linearly to final carbon content: at 65%, a 2% let-down puts 1.3% carbon in the wall. That predictability is the reason to buy carrier-free — but it also means an error in dosing shows up directly in the part, with no carrier phase absorbing the mistake. Gravimetric dosing on a carrier-free grade is worth the setup time.

65% versus the lower-loading routes to the same part

Three ways to reach a deep-black engineering part, and what each one costs you elsewhere.

RouteWhat enters the meltWhere it winsWhere it costs you
SY-65 (carrier-free, 65%)Carbon black + compounding aids onlyYour compound's HDT, impact and flow stay exactly as specified; deep jetness at low additionDemands proper drying, conveying and shear — the line has to be set up for it
Matched-carrier grade at 40%Carbon black + ABS/PS/PC carrierEasier processing on average equipmentCarrier enters your formulation and dilutes the properties you paid the resin for
Pre-compounded black resinFully formulated compoundSimplest at the machine — no dosing decisionsYou buy the black and the polymer together, at the compounder's price, and lose control of the formulation

The rule of thumb: the more of your part's performance is carried by the base resin, the more a carrier-free grade is worth. If you are moulding a technical part where impact and HDT were specified for a reason, adding a carrier phase to save a little processing convenience is a poor trade. If you are running commodity parts on average equipment, the matched-carrier or pre-compounded route will often be cheaper end to end.

Questions buyers ask about SY-65

Why carrier-free instead of a matched carrier?

For engineering resins, any added carrier phase dilutes the properties you pay for in ABS/PC. Carrier-free means the modification math stays yours.

Can it run in PA or PET?

The standard grade is validated on ABS/PS/PC. For PA, PET, PBT we compound carrier-matched systems — ask with your resin grade and target carbon.

What does 65% cost per part?

More per kg, less per part: at 1–2% let-down the finished-ton color cost usually beats a 40% grade. The quote shows both per-kg and per-finished-ton math.

How do I get a SY-65 sample and the full TDS?

Use the form below or email Zoe Lin with your polymer, process and target. The full SY-65 data sheet goes out the same day, and a free 2–5 kg line-trial sample follows — produced under the same compounding conditions as commercial batches.

Batch CoA on every shipment Free sample for line trial Your spec kept confidential 60,000 t/yr capacity

Get a SY-65 quote + TDS

Tell us your polymer, process and target carbon black in the part. We reply with the SY-65 spec sheet, a let-down recommendation and a firm factory quote.

You will hear back from Zoe Lin, our export manager, within one working day.

See the plant behind SY-65

SY-65 is compounded for conduit and profile applications. This is the compounding line and the QC laboratory.

Full factory tour — 2:50 on YouTube

Two minutes and fifty seconds inside the Huizhou plant: raw-material dosing, compounding, pelletising, packing and the QC laboratory.

Watch the full tour on YouTube →

Factory-direct. Annual capacity 60,000 t/yr. Certification details on the certifications page.